The Company that creates new value beyond t echnology
MS TECH CO., LTD.




| Number | Item | Test Method | Direction | Value |
|---|---|---|---|---|
| 1 | Weight | ASTM D 3776:2009, OPTION A : g/㎡ |
- | 115 |
| 2 | Tensile Strength | ASTM D 5035:2011, C.R.E. Strip Method: N/50mm |
MD | 488.4 |
| CD | 423.9 | |||
| 3 | Elongation | ASTM D 5035:2011, C.R.E. Strip Method: % |
MD | 18 |
| CD | 17.3 | |||
| 4 | Tear Strength | ASTM D 2261:2013, C.R.E. Blank: N |
MD | 124.1 |
| CD | 124.7 | |||
| 5 | Cold Resistance | ASTM D 6797:2015, C.R.E. Ball Busting Method: N |
- | 398 |
| 6 | Light Transmittance | ASTM E 424-71.:2007, Method A : 6.5.2, SELECTED ORDINATES Method : % |
white | 76.2 |
| Aluminum | 82.8 | |||
| 7 | 5000 hrs of UV Exposure |
ASTM D5035 : 2011 C.R.E, Strip Method : Retention rate % |
MD | 94 |
| CD | 94 |